activated zinc oxide

英 [ˈæktɪveɪtɪd zɪŋk ˈɒksaɪd] 美 [ˈæktɪveɪtɪd zɪŋk ˈɑːksaɪd]

网络  活性氧化锌

化学



双语例句

  1. A new technique for preparing activated zinc oxide with the ammonium chloride leach process has been developed.
    本文报道了利用氯化铵作为浸取剂,制备活性氧化锌的实验研究结果。
  2. Less amount of activated zinc oxide can be used for better efficeucy and it is suitable for food industry.
    活性氧化剂性能优良,可以减量使用,并能用于食品行业。
  3. The conclusion could be drawn that reducing the amount of activated zinc oxide was a reasonable measure.
    因此提出用活性氧化锌代替普通氧化锌时,减量是合理可行的措施。
  4. After reducing the activated zinc oxide amount, the experiments proved that the cure state and physical properties of cured rubber have not been impaired.
    并通过实验,证实减量后的活性氧化锌无论对硫化活性和硫化胶物性均无影响。
  5. Study on the preparation of activated zinc oxide from zinc oxide mine;
    研究用硫酸浸出锌浮渣制备超细活性氧化锌粉体的扩大试验。
  6. There are two main basical preparation methods of activated zinc oxide.
    我国传统的氧化锌生产方法主要是酸浸法和氨配合法。
  7. Activated zinc oxide is prepared by using zinc oxide ores as raw material through acid-leaching. purification and calcination operations.
    用氧化锌矿作原料经酸浸、净化和焙烧可制得纯度为98.3%的活性氧化锌,工艺简单。
  8. Preparation of Activated Zinc Oxide and Copper Sulfate from Spent Methanol Catalyst
    用废甲醇催化剂制备活性氧化锌和五水硫酸铜
  9. A new process which produce copper sulfate pentahydrate and activated zinc oxide from the used catalyst by soaking in complex acid has been introduced in this paper.
    本文介绍采用络合酸浸法以废甲醇催化剂为原料制备五水硫酸铜和活性氧化锌的新工艺。
  10. Investigation based on different kinds of amphoteric oxides such as activated alumina, molecular sieve of 4A type, activated silica, light magnesium oxide and activated zinc oxide was carried out.
    以γ-氧化铝、4A分子筛、活性二氧化硅、轻质氧化镁和活性氧化锌等两性氧化物用做催化剂进行研究。
  11. This paper introduces the process and principle of activated zinc oxide by full-wetting process from ore deposit as well as technical modification.
    介绍采用全湿法浸取低品位氧化矿生产活性氧化锌的生产工艺、原理及对传统活性氧化锌生产工艺的改进;
  12. This article introduce the principle, operation processes and conditions of production, all of which teach us how to use copper and zinc in dead methanol catalyst, in order to produce industrial copper sulfate and activated zinc oxide and by-product ammonium sulfate.
    介绍了利用氮肥厂废甲醇触媒中的铜、锌制取工业级硫酸铜和活性氧化锌并副产硫酸铵的原理、操作过程及条件。
  13. Material optimization of the reservoir in automatically activated zinc silver oxide primary battery
    自动激活锌-银储备电池用泡囊材料优选
  14. Effects of acid-leaching temperature and pH value on zinc leaching rate are studied. The impurities removal in the purification process and the effect of calcination process on preparation of activated zinc oxide are also examined.
    研究了酸浸温度、pH值对锌浸出率的影响,考察了净化工艺中的除杂问题,并用DTA分析了活性氧化锌制备过程中焙烧工艺的影响。
  15. Research on preparation of ultra-fine activated zinc oxide powder from zinc dross by nitric acid leaching
    硝酸浸出锌浮渣制取超细活性氧化锌的新工艺研究
  16. Dust of Snow Preparation of Activated Zinc Oxide from Arsenic Containing Crude Zinc Oxide
    利用含砷氧化锌尘制备活性氧化锌
  17. The nanometer characterization of activated zinc oxide was discussed in this paper.
    的纳米特性,从中得出减量应用的依据。
  18. A Study on Preparation of Chemical Manganese Dioxide and Activated Zinc Oxide in the Chlorhydric Acid Medium
    盐酸介质中制取化学二氧化锰与活性氧化锌的研究
  19. Qualified activated zinc oxide can be obtained by leaching out the arsenic from crude zinc oxide with NH 3 ( NH 4) SO 4 solution.
    用NH3-(NH4)2SO4溶液浸取处理含砷氧化锌尘,可彻底清除砷,制备出合格的活性氧化锌。
  20. With the demand for zinc oxide and the increasing awareness of environmental protection, the technology for preparation of activated zinc oxide from zinc blast-furnace ash and low-grade zinc oxide ore were taken seriously.
    随着氧化锌需求的持续增长和人们环境保护意识的增强,含锌烟尘等低品位氧化锌物料制备活性氧化锌的技术越来越受到重视。
  21. Ammonia complex method is an important technology on preparation of activated zinc oxide, which has the advantages of short flow, low costs.
    氨法制备活性氧化锌是碱法制备氧化锌中的一种重要的方法,其工艺流程简单,生产成本低。
  22. Besides, the preparation of activated zinc oxide by ammonia complex method has encounters many shortages, such as unstable quality of products, long reaction time and high energy-consuming.
    采用氨法制备活性氧化锌产品质量波动大,尚存在反应时间长,能耗高等不足。